15.
For an intaglio print use the natural bristle brush very gently
or use a cellulose sponge. After washing the plate for 30
seconds place the plate on a towel and examine the depth of
the wash-out. For an intaglio print an interrupted wash-out
is needed. This may be enough wash-out.
|

16.Printight,
Nyloprint, Miraclon and some other brands of photopolymer
plate require a softer brush or paint pad for the wash-out
than the natural bristle brush used on Torelief plates.
|
|

17.
After the required wash-out is achieved, wipe the plate surface
with a relatively dry sponge to remove any excess moisture
from the surface of the plate.
|

18.
Dry the surface of the plate with a fan heater or hair dryer
for 5 minutes on a warm setting.
|
|

19.
Post expose the plate for the same time as the first exposure
or until there are no sticky wash-out areas.
|

20.
Bevel the edge of an intaglio plate holding a design knife
at 45 degrees and cutting through the polymer. If the edge
needs evening up a fine file can be used.
|
|

21.
For an intaglio print, ink the plate using intaglio ink mixed
with Easy Wipe compound. Then wipe the plate using tarlatan
and phonebook paper.
|

22.
Print through an etching press on lightly dampened paper with
slightly less pressure than for printing metal plates.
|
|
|